So as to provide you with ease and enlarge our business, we even have inspectors in QC Crew and guarantee you our best company and solution for Concrete Surface Retarder , Frp Glass Fiber , Gfrc Glass Fiber , If you are interested in any products, please feel free to contact us for further information or please send us email directly, we will reply you within 24 hours and the best quotation will be provided.
Cheapest Price Gfrc Glass Fiber - Oil demolding agent – Xiangye Detail:

Usage Method

Dilution method: transfer the water to the desired concentration, and please stir well. The is diluted with clean water and sprayed on the surface of the mold. The specific dilution ratio of should be selected according to the difficulty of release molding of silicone products. Even the amount of release agent sprayed in the process of use will not cause bad appearance phenomena such as whitening, crack, watermark, oil and other surface of the product after forming oil release agent use method is simple, brush up directly, pouring concrete can be

Common problems encountered during the use of the mold release agent

1. Ineven injection- – - – - – - – - – - – - – - -improved coating

2. Spray flow- – - – - – -adjust the spraying amount

3. Wipe- – - – - – - – - – - – -select release agent hardness and solvent system

4. Evaporation- – - – - – - – - – - – - – -solid separation solubility or solvent solubility is different, orange peel phenomenon, evaporation when the solid precipitation can not form a uniform skin film, adjust the dispersant and solvent

5. Product shrinkage- – - – -shrinkage stress exceeds tension resistance, concentric marks, mainly choose material shrinkage, injection pressure and other adjustments

6. Bubble- – - – - – - – - – - -the product surface has many small bubble pits, raw material problems or release agent foaming performance, the gap between the release agent and mold into the air or the mold surface is rough, improve the hardness of release agent

7. Heat capacity of mold material- – - -mold reinforcing material heat capacity distribution is different, different heat storage, high temperature reaction is fast, or high temperature dissolution of mold release agent caused


Product detail pictures:

Cheapest Price  Gfrc Glass Fiber - Oil demolding agent – Xiangye detail pictures

Cheapest Price  Gfrc Glass Fiber - Oil demolding agent – Xiangye detail pictures

Cheapest Price  Gfrc Glass Fiber - Oil demolding agent – Xiangye detail pictures


Related Product Guide:

Our group through specialist training. Skilled expert knowledge, sturdy sense of assistance, to fulfill the provider needs of shoppers for Cheapest Price Gfrc Glass Fiber - Oil demolding agent – Xiangye , The product will supply to all over the world, such as: French, Slovak Republic, Algeria, Looking forward, we will keep pace with the times, continuing to create new products. With our strong research team, advanced production facilities, scientific management and top services, we will supply high quality products to our customers worldwide. We sincerely invite you to be our business partners for mutual benefits.
  • Hope that the company could stick to the enterprise spirit of "Quality, Efficiency, Innovation and Integrity", it will be better and better in the future.
    5 Stars By Julie from Houston - 2018.02.21 12:14
    The sales manager is very patient, we communicated about three days before we decided to cooperate, finally, we are very satisfied with this cooperation!
    5 Stars By Eric from Seattle - 2018.07.26 16:51